Finish was a horrifying combination of orange peel and sandpaper, in different spots. The ingredients mixed: Transtar 2K Kwik Prime and Transtar 2K Kwik Prime Activator. A review of instructions does allow for "up to" 1 part reducer. I originally didn't use reducer since the instructions on the previous Starlite SL-2K primer and SL-2K activator I was using noted to use reducer only if being used as a sealer (That primer job sucked too but I was attributing this new suck job more to the new gun and my inexperience with it). Things improved a little when I mixed in some Urethane Fast reducer, but by then most of the damage was done.

So... I've wet sanded it out with 220 and finished up with 600 grit but still have many pinpoint sized micro pits. Can I reshoot a few good coats and sand out or should I continue sanding MORE before shooting.

Thanks for the help. I seem to need it.

jmd_forest
__________________
86 944 NA - Brought back from the dead
Old 04-01-2008, 06:23 AM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #10 (permalink)