So....heating is next on the list
Hi All!
What is the best way to go about R&Ring my heating tubes and flapper boxes? Should I get them acid dipped and powercoated, or what would the peanut gallery recommend? b
__________________
According to Google, "I" am Mike Mueller ![]() 1974 914 with 72 1.7 and 74 L-Jet system (vroom) |
||
![]() |
|
Registered
Join Date: Oct 2002
Location: Tucson, AZ
Posts: 1,599
|
Probably bead blasting is better. I think acid is too corrosive and can damage metal parts. Powdercoating might work OK but could cause problems with the moving parts. Just a good quality high-temp paint is fine. Eastwood company sells some good stuff but the FLAPS stuff is probably fine also.
|
||
![]() |
|
Registered
|
i used slits beadblaster and cleaned them up real well for grimstead.
__________________
-Aaron "60% of the time, it works every time" |
||
![]() |
|
Registered
|
thanks guys...
i'll see if i can't find a beadblasting place in BG....or maybe i'll just sand the paint off and reapply it.... regardless, I think I have all of the pieces..... thank you for your help.... b