60/40 has been the standard for quite a while. While there are other combinations keep in mind that the tin(60%) is for strength/coductibilty and the lead (40%) is for flexibilty, as it's more pliable. Be sure to use Rosin core or a Rosin based flux.

As Matt suggests make a good solid, deep seated joint.