Quote:
Originally Posted by oldE View Post
OK, here's where I show off my incredible depth of ignorance.
I notice the blueing on the first two revolvers shown is not uniform. I understand that blueing is a chemical process and the final effect can depend upon a number of factors which may include surface preparation, strength of solution and temperature.
My question is : is the mottled effect desired on certain pieces?
The mottled effect that looks like an oil spill on water is actually color case hardening, not rust blueing. Involves heating and oil quenching.

For real differences, see https://www.africahunting.com/threads/color-case-hardening-vs-blueing.39031/


Personally, while I love nice wood and deep blue, I'm a "blank paint over parkerized metal" kinda guy