Orange peel is too much product and not enough air atomization. Get the tds for your paint and follow it. Pressure going into the gun should be between 25 ish depending on gun. Try using a 1.3 or 1.4 tip. Also when did you prime, did you use a sealer and if so what type. Your solvent pop could be coming from the sealer or primer underneath. If no luck let it dry sand with 1500 then 2000 and see if you can get rid of nubs. Sometimes you’ll get lucky and be able to sand them and buff them out.
|