Barry just got back to me, here is his reply.

Epoxy loves blasted metal and yes for 20 years said day with 80 but in the last few years my stand has been using coal slag or sand just clean with 700 and epoxy as sand leaves a nice anchor.
All other media must be da'ed with 80.


I then asked him if crushed glass was acceptable as well and he said yes.


Barry is a really good guy BTW. I owe him a lot.
I'm surprised he said crushed glass, that doesn't create a tooth, it creates dimples. Cerakote requires aluminum oxide to create a tooth and they say precisely not to use glass because it leaves a dimpled surface.

And I like a blasted surface because it gets everywhere, especially in little nooks and crannies that nothing else can, and in seams, an important place for adhesion.
__________________
Tru6 Restoration & Design

Last edited by Shaun @ Tru6; 11-07-2023 at 09:34 AM..
Old 11-07-2023, 09:31 AM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #12 (permalink)