Quote:
Originally Posted by Shaun @ Tru6
Thanks for the clarification. Agreed on the sand. I only use Al oxide for Cerakote work and send a body to NH for blasting. They use black beauty I think. The owner operator is a real life Flashdance character, wears a heavy respirated outfit, peels off her hood and it quite beautiful.
|
I got started using crushed glass because it was available locally and cheap. Black Beauty/Black Diamond is priced similar but for whatever reason I have never liked it as much. Lots of folks do though and get good results. Some of it may come down to the equipment that is being used. I have a decent but nowhere near top of the line pressure blaster. Maybe one day but the really good machines are $5K and up and hard to justify when only blasting 2 or 3 per year.
You do great work BTW. Have enjoyed reading your posts and seeing the results you get on stuff.