Back in the mid eighty's I worked in a boatyard that built multi million dollar luxury yachts.
The brother of one of the owners was hunting up in Alaska and lost a filling. He packed in
some Marine Tex epoxy and it lasted for decades. I had a acrylic dental partial that had cracked a
number of times. Kept taking it in to a great denturist who would repair it. Got tired of going
in so I have repaired it carefully with JB weld a number of times. Filed and sanded it to fit
properly and it kept in in good use for a number of years. Going in now to have a new metal
partial made with the same denturist,But the JB weld did work. My skill set did help. in knowing
what I was doing and being very careful re aligning the broken partial.
|