View Single Post
Pazuzu Pazuzu is online now
Registered
 
Join Date: Apr 2008
Location: Houston TX
Posts: 8,770
Use either high temp copper antisieze, or they make some $$$ stuff specifically for stainless fittings (we used lots of it when building a very complex hydrogen reactor once, HUNDREDS upon HUNDREDS of stainless bolts, nuts, and Swagelok fittings.

Swagelok Silver Goop (oh geeze, I didn't know it was THAT much money when we were using it!!!) One ounce, $200...

But, I'll tell ya, stainless to stainless and stainless to aluminum was painless, and never galled.
__________________
Mike Bradshaw

1980 911SC sunroof coupe, silver/black
Putting the sick back into sycophant!