The chips come off in chunks anywhere from .100" across to dust. It looks like very small Grape Nuts cereal.

The reason I mention cast iron is because our chips resemble the cast iron powdery type of chip and I figired there has to be a way already in use that keeps the very fine powdery type chips out of the coolant tank.

We have all the processing done and aren't having any trouble machining the material, it's keeping the powder out of the coolant tank that I am looking into.

We developed the material and machining process.