Any difference between....

The alloy used in the 1976 14X5.5 Fuchs and the alloy used in the ring type centre cap?

I have just spent the afternoon polishing a wheel and cap using the same methodology and grades of wet and dry, finishing off with Mother's.

The wheel is bright and shiny and almost a white colour, the centre cap is greyer and nowhere near as shiny. Still looks seriously Bling though.

Before anyone asks, yes I have got all the anodising off before starting the wet and dry process.

Any advice or similar experiences? Matt