One fender and rear bumper finally in primer. Its a little cold (52°) here in LA and I was a bit concerned about the primer curing properly in the cold weather but its only going to get colder so I decided to gamble and primer rather then risk exposing the bare metal until it warms up.
There is a little orange peel in the primer. Is this normal or are my gun settings wrong?
Prepping the bumper to weld up the exhaust hole:
Weld Finished and cleaned up. It was hell getting the fit right.... Front bumper was the donor metal:
Bumper in Primer, I think that will be ok...thoughts?