Quote:
Originally Posted by dfink
Sand_Man - Did you apply the hylomar to both sides of the case or did you use the 574 on the case and now plan to use the hylomar in the repair
|
I used the Threebond 1104 on my case halves...no issues there. A thin coat of 574 was used on many of the paper-like gaskets. Most are holding up fine, it's just the cam box areas that are in need of attention. It's nothing dramatic yet, but I know it's only a matter of time before the drops start. So these are the areas that I'll be using the Hylomar on.
__________________
-jeff
back in the saddle: '95 993 - just another black C2
*SOLD*: '87 930 GP White - heroin would have been a cheaper addiction...
"Ladies and Gentlemen, from Boston Massachusetts, we are Morphine, at your service..." - Mark Sandman (RIP
)