This is not the most current info..but I believe it to be still true.
Marine Ply and reg house ply uses the same glue. ( resourcenal)
The difference being is the quality of wood.
Marine is more plys and no blows
construction ply same glue, lower quality of wood and of course the blows.
You will have no problems.
If you keep the water out it will last for ever
There is NO such thing as dry rot
Rot is a fungus and operates best @ 50 % wet 50 % of the time.
__________________