Quote:
Originally Posted by Gregsgroup
one more question. Is Yamaha-bond and Three bond 1194 comparable? I plan on using the Yamaha bond for the case thru o-rings and was wondering if you can use it for the outer case. If so, I have an entire day to build my motor. Its about time 
|
No, don't use either. The o-rings need to be compliant to handle thermal expansion/contraction. Use Dow Corning 111 to lube the o-rings.