The refinishing process... Day 1

David sent this to me today...

as she was...


all apart...

I found out that she bites!

Into the acid tub to remove all the old blue.....

Scrubbed with bronze wool, rinsed, and blown dry.....

really bad pitting on the slide. I have seen this a lot in what I
call suicide guns. Usually blood pitting badly on only one
side.....This will be next to impossible to get flat without altering
the slide dimensions.

More pitting in the rear.... I think I'm gonna look for a good slide
for you....


Quick polish with a bronze wheel and into a plastic bag with some oil
spray. At this point it will rust in a matter of hours without oil.

More to come tomorrow.....

David


Needless to say, David found a replacement slide to replace the badly pitted one I had, so he ordered it for me. What a guy!! I can't wait to see what the old gun (mfg'd in 1924, I believe) will look like once David has finished his metallurgy magic!
__________________
Art Zasadny
1974 Porsche 911 Targa "Helga" (Sold, back home in Germany)
Learning the bass guitar
Driving Ford company cars now...
www.ford.com
Old 02-01-2011, 03:25 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #20 (permalink)