Nikasil is SiC embedded in a nickel matrix.

I would suggest that acid will not dissolve the hydrocarbon/varnish....it will etch (dissolve) the nickel (and any exposed aluminium) thereby lifting the glaze, further exposing the SiC thereby increasing surface roughness.