The plain bearing on the opposite end of the IMS would be lucky to see 10% of the ball bearing loads so there is no point in this comparison. Surface speeds of plain bearings are an issue with Aluminium a nickel bronze would be a better choice.
Nickel Bronze as well as other types of bronze materials proved unsuccessful in direct comparisons as materials for the IMS Solution.

Various diameters were also directly compared and nothing worked as well as the diameter that we chose. The load carrying capacity of a journal bearing isn't solely defined by diameter.



It is not the critic who counts; not the man who points out how the strong man stumbles, or where the doer of deeds could have done them better. The credit belongs to the man who is actually in the arena, whose face is marred by dust and sweat and blood; who strives valiantly; who errs, who comes short again and again, because there is no effort without error and shortcoming; but who does actually strive to do the deeds; who knows great enthusiasms, the great devotions; who spends himself in a worthy cause; who at the best knows in the end the triumph of high achievement, and who at the worst, if he fails, at least fails while daring greatly, so that his place shall never be with those cold and timid souls who neither know victory nor defeat.
Teddy Roosevelt
__________________
Jake Raby
Flat 6 Innovations and Aircooled Technology
IMS Solution Inventor
US Patents:8,992,089/ 9,416,697/ 9,687,974/ 9,909,369
'64 356C Outlaw,'76 912E,95’ 993,89’ 964 &'88 Carrera
Old 01-30-2014, 05:39 AM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #244 (permalink)