My only painting experience is with bicycles... but ... sandblast, acid bath, neutralize acid, zinc chromate primer, du pont imron from 6 different angles (needed for tube shape for correct coverage w/ no runs), clear coat, let harden under slightly warm lights (about 100 degrees).
Depending on how bad the bubbling is, you may be able to get away with something like wet sanding and then a clear coat... but I doubt it. Of course, if you take it down to bare metal, color matching may be problematic...
A local body shop could probably do it good for you for under $500....