Quote:
Originally Posted by bugstrider View Post
I have been told that post baking immediately following the plating process corrects this issue.
Yes... I have to get some aviation parts zinc plated and they must be baked right after the plating. This takes care of the problem, but it is an additional process at an additional cost.