I have used lots of Lithium.
Assuming floor has no curing agent or sealer. Scrub floor with water to clean. Let dry as long as possible. A couple of days is great.
Apply one coat of Llithium. Depending on the temperature and humidity, apply second coat a few hours later.
Ideally you want to apply it at 1000 square feet per gallon per coat.
The next day, buff with high-speed buffer ( 1500-2500 rpm) and burnishing pad.
This is a NAPA Auto Parts that we did earlier this year with Lithium.