re-ringing a 2.7. hone or not to hone.
I am rebuilding a 2.7. the compression was good on the old engine, but I am going to rering it anyways. should I rough up the cylinders or leave them as is when I rering it? what do ya'll think...
|
||
![]() |
|
Registered
|
Nickasil or Alusil P&Cs?
__________________
'76 911 Carrera 3.0 |
||
![]() |
|
Registered
Join Date: Dec 2002
Posts: 9
|
nikasil cylinders.
|
||
![]() |
|
Registered
|
Others may chime in since this is a somewhat controvercial topic. I believe Henry Schmidt at Supertek recommends that you lightly scuff them up with a scotchbrite pad in soap and water. That's what I did when re-ringing my Nickasils. Seems like the rings seated fine.
Others may say to just leave them alone. My exeperience is very limited, but it seems to have worked for me.
__________________
'76 911 Carrera 3.0 |
||
![]() |
|
Registered
Join Date: Sep 1999
Location: Featherston, New Zealand
Posts: 962
|
Plenty of food for thought here----
Re-ring Alusils? |
||
![]() |
|