			Does anyone know of any product you could use to cast small parts originally made from Bakelite? Something with some strength that would take higher temps. Just wondering... 
				__________________ Steve B. 1971 T 2.2 w/Zeniths Gruppe B member 171 Mid 9 Web Site Guy | ||
|  08-29-2005, 04:12 AM | 
 | 
| Registered Join Date: Sep 2002 
					Posts: 513
				 | 
			If it is ok to be conductive metal you could get a simple sand-casting kit used to make jewelry(I think mine was less than $50).  The casting grains are very inexpensive.
		 | ||
|  08-29-2005, 04:26 AM | 
 | 
| Registered | 
				__________________ Warren & Ron, may you rest in Peace. | ||
|  08-29-2005, 05:36 AM | 
 | 
| Registered | 
			It does have to be non-conductive. Should have said that.
		 
				__________________ Steve B. 1971 T 2.2 w/Zeniths Gruppe B member 171 Mid 9 Web Site Guy | ||
|  08-29-2005, 05:52 AM | 
 | 
| Registered | 
			Devcon makes liquid plastic.
		 
				__________________ 2014 Cayman S (track rat w/GT4 suspension) 1979 930 (475 rwhp at 0.95 bar) | ||
|  08-29-2005, 05:54 AM | 
 | 
| Registered | 
			Does anyone know if fiberglass resin can take any heat. I'm thinking specifically of reproducing Beru connector tubes. I was wondering about tiger hair???
		 
				__________________ Steve B. 1971 T 2.2 w/Zeniths Gruppe B member 171 Mid 9 Web Site Guy | ||
|  08-29-2005, 06:01 AM | 
 | 
|   | 
| Registered | 
			Fiberglass resin, at least the boat stuff I've used, is very brittle.  The Devcon stuff is very good, we use it at work.  You can use it to make molds and then with a release agent you can make parts in the molds.
		 