Help: Targa bar primer adhesion problem

I've removed my Targa bar cover, used a stripper to remove most of the black paint, and wet sanded to remove the rest. Today, I cleaned it with thinner and dried off with paper towels. I then sprayed a thin coat of Wurth self-etching primer in the basement of the pool house (relatively high humidity), and then brought it upstairs to dry (lower humidity). After about half hour, I went to check on it and found that in certain spots, the primer was chipping off with no adhesion of any primer to the bare bar. The location of this chipping is limited to the front vertical surface with the screw holes, but only in a few spots. There is no such chipping on any other surface of the Targa bar. This leads me to believe that the chipping is not due to the humidity present while spraying.

Any thoughts about the cause of this chipping or, more importantly, how to get the primer to stick to the Targa bar at those spots?

Thanks,

Steve

Old 06-08-2013, 12:36 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #1 (permalink)
ROW '78 911 Targa
 
timmy2's Avatar
 
Join Date: Jul 2011
Location: Salem, OR
Posts: 10,214
Garage
Usually it's a problem with a layer of dirt or something on the metal that stops adhesion.
Try sanding and really cleaning the problem areas and hit them with primer again.
__________________
Dennis
Euro 1978 SC Targa, SSI's, Dansk 2/1, PMO ITBs, Electric A/C
Need a New Wiring Harness? PM or e-mail me. Search for "harnesses" in the classifieds.
Old 06-08-2013, 01:41 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #2 (permalink)
Registered User
 
Michael T's Avatar
 
Join Date: Jan 2011
Location: Houston
Posts: 237
It is likely the high humidity when the primer was sprayed. I live in Houston and after two attempts in June and then August, the humidity was just too high. When I waited to October and got a lower humidity and temperature, it looked great. No change in technique.
Old 06-08-2013, 01:53 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #3 (permalink)
Registered
 
Justin@Athens's Avatar
 
Join Date: Jun 2009
Location: Athens, GA
Posts: 1,206
Garage
Send a message via AIM to Justin@Athens
Any residue left from the acetone would cause this. Because you mention that is in select locations, along the same surface, this leads me to believe you may have simply neglected to wipe down this area as well as the rest of the piece.
__________________
1990 964 C4 Coupe & 1991 964 C2 Coupe (current)
1989 911 Targa (sold)
1996 993 Cab. (sold)
1999 x2 Boxster (sold)
2006 Cayman S (my daily)
Old 06-08-2013, 02:02 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #4 (permalink)
Registered
 
porwolf's Avatar
 
Join Date: May 2011
Posts: 7,245
I never painted a Targa bar but I have some experience with 2 component epoxy. Maybe you could strip the bar again, new paint should come off easily, clean sand paper the front edge thoroughly and brush on regular epoxy. Epoxy really adheres well to stainless steel, especially when it is not a smooth surface. After the epoxy cures you could sand that smooth and apply regular paint. Like I said, I have not done that, just a thought.
__________________
79 SC Targa
72 T Targa Sold
68 T Coupe Sold
65 912 Coupe Sold
62 356B Coupe Sold
Old 06-08-2013, 02:10 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #5 (permalink)
Reiver
 
Reiver's Avatar
 
Join Date: Nov 2011
Posts: 57,376
Have you thought about getting a wrap on it? It seems that particular piece would be easy and low maint.
Old 06-08-2013, 02:22 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #6 (permalink)
Registered
 
Join Date: Dec 2008
Location: San Antonio, Texas
Posts: 3,590
powdercoat is the most durable.
__________________
1973 911S (since new) RS MFI specs
1991 C2 Turbo
Old 06-08-2013, 05:48 PM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #7 (permalink)
Registered
 
Join Date: Feb 2013
Location: Allendale, New Jersey
Posts: 122
Garage
All: Thank you for your prompt and helpful responses. This morning, I removed all of the primer by wet sanding. Then I wiped down with thinner and dried and then cleaned again with Clorox wet wipes for stainless steel and dried, and then dried in sun. Applied a coat of primer on back lawn in the sun and then placed in pool house to dry. After two hours, the primer adhered in all locations. Thank you again.

Steve

Old 06-09-2013, 08:53 AM
  Pelican Parts Catalog | Tech Articles | Promos & Specials    Reply With Quote #8 (permalink)
Reply

Thread Tools
Rate This Thread
Rate This Thread:

 


All times are GMT -8. The time now is 01:58 AM.


 
Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2025, vBulletin Solutions, Inc.
Search Engine Optimization by vBSEO 3.6.0
Copyright 2025 Pelican Parts, LLC - Posts may be archived for display on the Pelican Parts Website -    DMCA Registered Agent Contact Page
 

DTO Garage Plus vBulletin Plugins by Drive Thru Online, Inc.